The data below were obtained from a creep test performed atroom temperature on a wire composed of 40% tin, 60% lead, andsolid core solder. This was done by measuring the increase in strainover time while a constant load was applied to a test specimen. Using a linear regression method, find (a ) the equation of these line that bestfits these data and (b ) the
If the line does not pass through the origin, force it to do so. Does thisnew line represent the data trend? Suggest a new equation that satisfies zero strain at zero time and also represents the data trend well.
Want to see the full answer?
Check out a sample textbook solutionChapter 20 Solutions
Numerical Methods For Engineers, 7 Ed
- Algebra & Trigonometry with Analytic GeometryAlgebraISBN:9781133382119Author:SwokowskiPublisher:CengageGlencoe Algebra 1, Student Edition, 9780079039897...AlgebraISBN:9780079039897Author:CarterPublisher:McGraw HillAlgebra and Trigonometry (MindTap Course List)AlgebraISBN:9781305071742Author:James Stewart, Lothar Redlin, Saleem WatsonPublisher:Cengage Learning
- Functions and Change: A Modeling Approach to Coll...AlgebraISBN:9781337111348Author:Bruce Crauder, Benny Evans, Alan NoellPublisher:Cengage Learning