What are galvanic corrosion problems common when discrete fasteners are used?

Blurred answer
Students have asked these similar questions
CORRECT AND DETAILED SOLUTION WITH FBD ONLY. I WILL UPVOTE THANK YOU. CORRECT ANSWER IS ALREADY PROVIDED. I REALLY NEED FBD. The cantilevered spandrel beam shown whose depth tapers from d1 to d2, has a constant width of 120mm. It carries a triangularly distributed end reaction.Given: d1 = 600 mm, d2 = 120 mm, L = 1 m, w = 100 kN/m1. Calculate the maximum flexural stress at the support, in kN-m.2. Determine the distance (m), from the free end, of the section with maximum flexural stress.3. Determine the maximum flexural stress in the beam, in MPa.ANSWERS: (1) 4.630 MPa; (2) 905.8688 m; (3) 4.65 MPa
CORRECT AND DETAILED SOLUTION WITH FBD ONLY. I WILL UPVOTE THANK YOU. CORRECT ANSWER IS ALREADY PROVIDED. I REALLY NEED FBD A concrete wall retains water as shown. Assume that the wall is fixed at the base. Given: H = 3 m, t = 0.5m, Concrete unit weight = 23 kN/m3Unit weight of water = 9.81 kN/m3(Hint: The pressure of water is linearly increasing from the surface to the bottom with intensity 9.81d.)1. Find the maximum compressive stress (MPa) at the base of the wall if the water reaches the top.2. If the maximum compressive stress at the base of the wall is not to exceed 0.40 MPa, what is the maximum allowable depth(m) of the water?3. If the tensile stress at the base is zero, what is the maximum allowable depth (m) of the water?ANSWERS: (1) 1.13 MPa, (2) 2.0 m, (3) 1.20 m
CORRECT AND DETAILED SOLUTION WITH FBD ONLY. I WILL UPVOTE THANK YOU. CORRECT ANSWER IS ALREADY PROVIDED. I NEED FBD A short plate is attached to the center of the shaft as shown. The bottom of the shaft is fixed to the ground.Given: a = 75 mm, h = 125 mm, D = 38 mmP1 = 24 kN, P2 = 28 kN1. Calculate the maximum torsional stress in the shaft, in MPa.2. Calculate the maximum flexural stress in the shaft, in MPa.3. Calculate the maximum horizontal shear stress in the shaft, in MPa.ANSWERS: (1) 167.07 MPa; (2) 679.77 MPa; (3) 28.22 MPa

Chapter 39 Solutions

DeGarmo's Materials and Processes in Manufacturing

Ch. 39 - How can the use of hot-melt adhesives be combined...Ch. 39 - What property enhancement characteristic is...Ch. 39 - What features or properties are provided or...Ch. 39 - What are some types of nonstructural or special...Ch. 39 - How can polymeric adhesives he made electrically...Ch. 39 - What types of radiation can be used with...Ch. 39 - What are some of the temperature considerations...Ch. 39 - What are some of the environmental conditions that...Ch. 39 - What is the difference between a...Ch. 39 - Why is it desirable for adhesive joints to be...Ch. 39 - Why are butt joints unattractive for adhesive...Ch. 39 - What types of joints provide large bonding areas?Ch. 39 - How does the strength of an adhesive joint vany...Ch. 39 - What are some common techniques by which surfaces...Ch. 39 - How can destructive testing and the examination of...Ch. 39 - Why are the structural adhesives an attractive...Ch. 39 - In view of the relatively low strengths of the...Ch. 39 - Why might an adhesive joint provide enhanced...Ch. 39 - What are some of the other attractive properties...Ch. 39 - In what ways might a structural adhesive offer...Ch. 39 - Why are adhesive joints unattractive for...Ch. 39 - Describe some of the ways that structural...Ch. 39 - What are some other common limitations to...Ch. 39 - What is weld bonding?Ch. 39 - What are some common types of mechanical...Ch. 39 - What factors would influence the selection of a...Ch. 39 - What types of fasteners are attractive if the...Ch. 39 - What factors determine the overall effectiveness...Ch. 39 - What is an integral fastener? Provide an example.Ch. 39 - What are some of the primary types of discrete...Ch. 39 - Prob. 41RQCh. 39 - What are some of the major assets of mechanical...Ch. 39 - What are some of the ways that fastener holes can...Ch. 39 - What is the benefit of a self-tapping fastener?Ch. 39 - What are some of the common causes for failure of...Ch. 39 - What are galvanic corrosion problems common when...Ch. 39 - From a manufacturing viewpoint, why is it...Ch. 39 - What are some of the ways that plastics can be...Ch. 39 - Why can the thermoplastic polymers be welded, but...Ch. 39 - Prob. 50RQCh. 39 - Describe several of the plastic joining processes...Ch. 39 - Prob. 52RQCh. 39 - How can metal inserts be used to produce welds in...Ch. 39 - Prob. 54RQCh. 39 - What is the difference between direct laser...Ch. 39 - Give an everyday example of solvent welding.Ch. 39 - What material property enables snap-fits to be a...Ch. 39 - Why are the crystalline ceramic materials...Ch. 39 - Prob. 59RQCh. 39 - Prob. 60RQCh. 39 - When materials are joined, interfaces are created...Ch. 39 - Some automakers are using adhesives and sealants...Ch. 39 - Select two types of additives to industrial...Ch. 39 - Identify at least five types of adhesives that...Ch. 39 - A contractor has installed aluminum siding on a...Ch. 39 - Mechanical fasteners are an attractive means of...Ch. 39 - Prob. 6PCh. 39 - Prob. 7PCh. 39 - Prob. 8PCh. 39 - Prob. 9PCh. 39 - Prob. 10PCh. 39 - You must devise a means of incorporating the...Ch. 39 - An additional joint occurs where the club head is...Ch. 39 - For production simplicity, it might be preferable...Ch. 39 - If the bonding process and resulting interface...Ch. 39 - Prob. 5CSCh. 39 - Prob. 6CS

Additional Engineering Textbook Solutions

Find more solutions based on key concepts
Knowledge Booster
Background pattern image
Mechanical Engineering
Learn more about
Need a deep-dive on the concept behind this application? Look no further. Learn more about this topic, mechanical-engineering and related others by exploring similar questions and additional content below.
Similar questions
SEE MORE QUESTIONS
Recommended textbooks for you
Text book image
Welding: Principles and Applications (MindTap Cou...
Mechanical Engineering
ISBN:9781305494695
Author:Larry Jeffus
Publisher:Cengage Learning
Stresses Due to Fluctuating Loads Introduction - Design Against Fluctuating Loads - Machine Design 1; Author: Ekeeda;https://www.youtube.com/watch?v=3FBmQXfP_eE;License: Standard Youtube License